General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Density of 8.8 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 115 GPa Show Supplier Material materials with Elastic modulus of 115 GPa |
Elongation A5 | 23.0 °C | 6 % Show Supplier Material materials with Elongation A5 of 6 % |
Hardness, Brinell | 23.0 °C | 220 [-] Show Supplier Material materials with Hardness, Brinell of 220 [-] |
Tensile strength | 23.0 °C | 690 MPa Show Supplier Material materials with Tensile strength of 690 MPa |
Yield strength Rp0.2 | 23.0 °C | 640 MPa Show Supplier Material materials with Yield strength Rp0.2 of 640 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.85E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.85E-5 1/K |
Thermal conductivity | 23.0 °C | 67 W/(m·K) Show Supplier Material materials with Thermal conductivity of 67 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 7.50E+6 S/m Show Supplier Material materials with Electrical conductivity of 7.50E+6 S/m |
Chemical properties
Property | Value |
---|---|
Copper | 89.8 - 93 % Show Supplier Material materials with Copper of 89.8 - 93 % |
Iron | 0 - 0.1 % Show Supplier Material materials with Iron of 0 - 0.1 % |
Other | 0 - 0.5 % Show Supplier Material materials with Other of 0 - 0.5 % |
Phosphorus | 0.03 - 0.35 % Show Supplier Material materials with Phosphorus of 0.03 - 0.35 % |
Tin | 7 - 9 % Show Supplier Material materials with Tin of 7 - 9 % |
Zinc | 0 - 0.2 % Show Supplier Material materials with Zinc of 0 - 0.2 % |