General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 7.8 g/cm³ Show Supplier Material materials with Density of 7.8 g/cm³ at 23.0 °C | 23.0 °C | typical for steels |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 200 - 210 GPa Show Supplier Material materials with Elastic modulus of 200 - 210 GPa at 23.0 °C | 23.0 °C | typical for steels |
Elongation A5 | 10 % Show Supplier Material materials with Elongation A5 of 10 % at 23.0 °C | 23.0 °C | |
Hardness, Brinell | 570 [-] Show Supplier Material materials with Hardness, Brinell of 570 [-] at 23.0 °C | 23.0 °C | |
Tensile strength | 1300 - 1500 MPa Show Supplier Material materials with Tensile strength of 1300 - 1500 MPa at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Carbon | 0.15 % | max. |
Chromium | 16 - 19 % | |
Manganese | 2 % | max. |
Molybdenum | 0.8 % | |
Nickel | 6 - 9.5 % | |
Silicon | 2 % | max. |