Description

Very good corrosion resistance, weldability and cold deformability. Good deep drawing properties and very good high gloss polishability.

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Supplier Material materials with Density of 7.8 g/cm³

typical for steels

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa

typical for steels

Elongation A5

23.0 °C

35 - 45 %

Show Supplier Material materials with Elongation A5 of 35 - 45 %

Hardness, Brinell

23.0 °C

215 [-]

Show Supplier Material materials with Hardness, Brinell of 215 [-]

Tensile strength

23.0 °C

500 - 700 MPa

Show Supplier Material materials with Tensile strength of 500 - 700 MPa

Yield strength Rp0.2

23.0 °C

190 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 190 MPa

Chemical properties

PropertyValueComment

Carbon

0.07 %

Show Supplier Material materials with Carbon of 0.07 %

max.

Chromium

17.5 - 19.5 %

Show Supplier Material materials with Chromium of 17.5 - 19.5 %

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

max.

Nickel

8 - 10.5 %

Show Supplier Material materials with Nickel of 8 - 10.5 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %