Chemical properties

Property

Boron

1.5E-3 - 5E-3 %

Carbon

0.04 %

Chromium

16 - 18.5 %

Iron

61.2 - 71.9 %

Manganese

2 %

Molybdenum

2 - 3 %

Nickel

10 - 14 %

Nitrogen

0.1 - 0.22 %

Phosphorus

0.05 %

Silicon

1 %

Sulfur

0.03 %