Stainless Steel 253MA

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Carbon

0.05 - 0.12 %

Show Supplier Material materials with Carbon of 0.05 - 0.12 %

Cerium

0.03 - 0.08 %

Show Supplier Material materials with Cerium of 0.03 - 0.08 %

Chromium

20 - 22 %

Show Supplier Material materials with Chromium of 20 - 22 %

Iron

62 - 68.4 %

Show Supplier Material materials with Iron of 62 - 68.4 %

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Nickel

10 - 12 %

Show Supplier Material materials with Nickel of 10 - 12 %

Nitrogen

0.12 - 0.2 %

Show Supplier Material materials with Nitrogen of 0.12 - 0.2 %

Phosphorus

0 - 0.05 %

Show Supplier Material materials with Phosphorus of 0 - 0.05 %

Silicon

1.4 - 2.5 %

Show Supplier Material materials with Silicon of 1.4 - 2.5 %

Sulfur

0 - 0.03 %

Show Supplier Material materials with Sulfur of 0 - 0.03 %