Titanium Grade 2

Alternative and trade names
Ti2
Want to keep this datasheet? Save it now in your required format

Description

This is the most widely used titanium quality with perfect weldability and is easily deformable. Application especially in the chemical industry, equipment construction, sports articles and jewelry.

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

23.0 °C

20 - 24 %

Show Supplier Material materials with Elongation A5 of 20 - 24 %

Hardness, Brinell

23.0 °C

190 [-]

Show Supplier Material materials with Hardness, Brinell of 190 [-]

Tensile strength

23.0 °C

345 - 450 MPa

Show Supplier Material materials with Tensile strength of 345 - 450 MPa

Yield strength Rp0.2

23.0 °C

275 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 275 MPa

Chemical properties

PropertyValue

Carbon

0.08 %

Show Supplier Material materials with Carbon of 0.08 %

Hydrogen

0.02 %

Show Supplier Material materials with Hydrogen of 0.02 %

Iron

0.3 %

Show Supplier Material materials with Iron of 0.3 %

Nitrogen

0.03 %

Show Supplier Material materials with Nitrogen of 0.03 %

Oxygen

0.25 %

Show Supplier Material materials with Oxygen of 0.25 %

Titanium

Balance