Titanium Grade 5

Alternative and trade names
Ti6Al4V
Want to keep this datasheet? Save it now in your required format

Description

Unlike grade 2, 3.7165 is heat-treatable and can be used at temperatures up to 400 °C. Mainly used in the medical and aerospace industries

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

23.0 °C

10 - 18 %

Show Supplier Material materials with Elongation A5 of 10 - 18 %

Hardness, Brinell

23.0 °C

370 [-]

Show Supplier Material materials with Hardness, Brinell of 370 [-]

Tensile strength

23.0 °C

900 - 990 MPa

Show Supplier Material materials with Tensile strength of 900 - 990 MPa

Yield strength Rp0.2

23.0 °C

830 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 830 MPa

Chemical properties

PropertyValue

Aluminium

5.5 - 6.7 %

Show Supplier Material materials with Aluminium of 5.5 - 6.7 %

Titanium

Balance

Vanadium

3.5 - 4.5 %