Invar 36

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.1 g/cm³

Show Supplier Material materials with Density of 8.1 g/cm³

Chemical properties

PropertyValueComment

Carbon

0.05 %

Show Supplier Material materials with Carbon of 0.05 %

max.

Iron

balance

Manganese

0.5 %

Show Supplier Material materials with Manganese of 0.5 %

max.

Nickel

35 - 37 %

Show Supplier Material materials with Nickel of 35 - 37 %

Silicon

0.3 %

Show Supplier Material materials with Silicon of 0.3 %

max.