General
Property | Value | Comment |
---|---|---|
Recycled Content | 82.1 % Show Supplier Material materials with Recycled Content of 82.1 % | Average recycled content |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 35 % Show Supplier Material materials with Elongation of 35 % | min. |
Tensile strength | 23.0 °C | 550 - 750 MPa Show Supplier Material materials with Tensile strength of 550 - 750 MPa | |
Yield strength Rp0.2 | 23.0 °C | 270 MPa Show Supplier Material materials with Yield strength Rp0.2 of 270 MPa | min. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbon | 0.03 % Show Supplier Material materials with Carbon of 0.03 % | max. | |
Chromium | 18.5 % Show Supplier Material materials with Chromium of 18.5 % | ||
Iron | Balance | ||
Manganese | 1.3 % Show Supplier Material materials with Manganese of 1.3 % | ||
Nickel | 9 % Show Supplier Material materials with Nickel of 9 % | ||
Nitrogen | 0.14 % Show Supplier Material materials with Nitrogen of 0.14 % | ||
Phosphorus | 0.04 % Show Supplier Material materials with Phosphorus of 0.04 % | max. | |
Silicon | 0.4 % Show Supplier Material materials with Silicon of 0.4 % | ||
Sulfur | 0.03 % Show Supplier Material materials with Sulfur of 0.03 % | max. |