General
Property | Value | Comment |
---|---|---|
Recycled Content | 82.1 % Show Supplier Material materials with Recycled Content of 82.1 % | Average recycled content |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 35 % Show Supplier Material materials with Elongation of 35 % | min. |
Tensile strength | 23.0 °C | 510 - 690 MPa Show Supplier Material materials with Tensile strength of 510 - 690 MPa | |
Yield strength Rp0.2 | 23.0 °C | 205 MPa Show Supplier Material materials with Yield strength Rp0.2 of 205 MPa | min. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbon | 0.06 % Show Supplier Material materials with Carbon of 0.06 % | max. | |
Chromium | 16.5 % Show Supplier Material materials with Chromium of 16.5 % | ||
Iron | Balance | ||
Manganese | 1.3 % Show Supplier Material materials with Manganese of 1.3 % | ||
Nickel | 13 % Show Supplier Material materials with Nickel of 13 % | ||
Niobium | 0.7 % Show Supplier Material materials with Niobium of 0.7 % | ||
Phosphorus | 0.02 % Show Supplier Material materials with Phosphorus of 0.02 % | max. | |
Silicon | 0.4 % Show Supplier Material materials with Silicon of 0.4 % | ||
Sulfur | 0.015 % Show Supplier Material materials with Sulfur of 0.015 % | max. |