PPS CF40 SGC401LFRT

Alternative and trade names
PPS-SGC401LFRT
Want to keep this datasheet? Save it now in your required format

Description

It is a 40% long carbon fiber reinforced linear polyphenylene sulfide with high toughness and high dimensional stability.

This material data has been provided by Sciengy New Materials Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.65 g/cm³

Show Supplier Material materials with Density of 1.65 g/cm³

ISO 1183

Water absorption

23.0 °C

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

ISO 62

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

0.55 %

Show Supplier Material materials with Elongation of 0.55 %

ISO 527

Flexural modulus

23.0 °C

35 GPa

Show Supplier Material materials with Flexural modulus of 35 GPa

ISO 178

Flexural strength

23.0 °C

340 MPa

Show Supplier Material materials with Flexural strength of 340 MPa

ISO 178

Impact strength, Charpy notched

23.0 °C

16 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m²

ISO 179

Tensile strength

23.0 °C

190 MPa

Show Supplier Material materials with Tensile strength of 190 MPa

ISO 527

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

280 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 280 °C

ISO 75

Flammability

V-0, UL-94

Technological properties

Property
Application areas

Can be used in vacuum pump impeller,oilfield accessories and other components

Fillers

40% Carbon Fiber

Processing methods

Injection Moulding / Test Specimen Production: Drying: 150°C & 3 hours - Injection Pressure: 30-100 MPa - Injection Molding Melt Temperature: 290-330°C - Injection Molding Mold Temperature: 120-160°C - Limit in-cylinder Retention Time: 300°C/60min or 320°C/30min