PEEK GF30 SG301A87

Alternative and trade names
PEEK-SG301A87
Want to keep this datasheet? Save it now in your required format

Description

It is a 30% glass fiber reinforced PEEK compound developed to provide toughness, temperature, chemical resistance and high strength.

This material data has been provided by Sciengy New Materials Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.51 g/cm³

Show Supplier Material materials with Density of 1.51 g/cm³

ISO 1183

Water absorption

23.0 °C

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

ISO 62

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2.7 %

Show Supplier Material materials with Elongation of 2.7 %

ISO 527

Flexural modulus

23.0 °C

11.3 GPa

Show Supplier Material materials with Flexural modulus of 11.3 GPa

ISO 178

Flexural strength

23.0 °C

270 MPa

Show Supplier Material materials with Flexural strength of 270 MPa

ISO 178

Impact strength, Charpy notched

23.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179

Tensile strength

23.0 °C

180 MPa

Show Supplier Material materials with Tensile strength of 180 MPa

ISO 527

Thermal

PropertyTemperatureValueComment

Heat deflection temperature, 1.80 MPa

330 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 330 °C

ISO 75

Melting point

343 °C

Show Supplier Material materials with Melting point of 343 °C

ISO 11357 (10°C/min)

Thermal conductivity

23.0 °C

0.3 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.3 W/(m·K)

ISO 22007-4

Flammability

V-0, UL-94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

150 V

Show Supplier Material materials with Comparative tracking index of 150 V

IEC 60112

Dielectric constant

23.0 °C

3.2 [-]

Show Supplier Material materials with Dielectric constant of 3.2 [-]

IEC 60250

Dielectric strength

23.0 °C

25 kV/mm

Show Supplier Material materials with Dielectric strength of 25 kV/mm

IEC 60243

Dissipation factor

23.0 °C

5E-3 [-]

Show Supplier Material materials with Dissipation factor of 5E-3 [-]

IEC 60250

Volume resistivity

23.0 °C

1.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm

IEC 60093

Technological properties

Property
Application areas

Chemical pump pump body and impeller, cable plug, junction box, ultra pure water system pipe fittings and valves.Engine bearing, shim, sealing element, clutch ring.The driving and brake parts of a car. Cable, wire, coil skeleton, connector, etc

Fillers

30% Glass Fiber

Processing methods

Extrusion or Injection Moulding / Test Specimen Production: Drying 150°C & 3 hours/120°C & 5 hours - Injection molding melt temperature: 360-385°C - Injection molding mold temperature: 180-200°C