PEEK CF30 SGC301ATF

Alternative and trade names
PEEK-SGC301ATF
Want to keep this datasheet? Save it now in your required format

Description

It is a 30% carbon fiber reinforced PEEK compound developed to provide higher strength, wear resistance, low coefficient of friction and chemical resistant.

This material data has been provided by Sciengy New Materials Co. Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.4 g/cm³

Show Supplier Material materials with Density of 1.4 g/cm³

ISO 1183

Water absorption

23.0 °C

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

ISO 62

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.5 %

Show Supplier Material materials with Elongation of 1.5 %

ISO 527

Flexural modulus

23.0 °C

25.5 GPa

Show Supplier Material materials with Flexural modulus of 25.5 GPa

ISO 178

Flexural strength

23.0 °C

380 MPa

Show Supplier Material materials with Flexural strength of 380 MPa

ISO 178

Impact strength, Charpy notched

23.0 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO 179

Tensile strength

23.0 °C

250 MPa

Show Supplier Material materials with Tensile strength of 250 MPa

ISO 527

Thermal

PropertyTemperatureValueComment

Heat deflection temperature, 1.80 MPa

335 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 335 °C

ISO 75

Melting point

343 °C

Show Supplier Material materials with Melting point of 343 °C

ISO 11357 (10°C/min)

Thermal conductivity

23.0 °C

1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1 W/(m·K)

ISO 22007-4

Flammability

V-0, UL-94

Electrical

PropertyTemperatureValueComment

Volume resistivity

23.0 °C

100000 Ω·cm

Show Supplier Material materials with Volume resistivity of 100000 Ω·cm

IEC 60093

Technological properties

Property
Application areas

Chemical pump pump body and impeller, cable plug, junction box, ultra pure water system pipe fittings and valves.Engine bearing, shim, sealing element, clutch ring.The driving and brake parts of a car. Cable, wire, coil skeleton, connector, etc

Fillers

30% Carbon Fiber

Processing methods

Extrusion or Injection Moulding / Test Specimen Production: Drying 150°C & 3 hours/120°C & 5 hours - Injection molding melt temperature: 375-395°C - Injection molding mold temperature: 180-210°C