HMPL.M BOPP (Biaxially Oriented Polypropylene) Metallized Film

Want to keep this datasheet? Save it now in your required format

Description

Metallized heat sealable BOPP film with a low sealing intention temperature and standard coefficient of friction for printing and lamination. The benefits are: Good adhesion of the aluminum layer; excellent optical and barrier properties of the metallized films; low threshold for welding, high adhesion of aluminum, good mechanical properties; stable standard coefficient of friction; contains slip-antiblock additives; intended for contact with food; without coatings and primers; UT side is allowed to accept activation inline on the printing press or laminator (if necessary).

This material data has been provided by SIBUR.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Thickness

0.02 - 0.04 mm

Show Supplier Material materials with Thickness of 0.02 - 0.04 mm

General

PropertyTemperatureValueComment

Density

20.0 °C

0.91 g/cm³

Show Supplier Material materials with Density of 0.91 g/cm³

Film yield

20.0 °C

27.47 - 73.26 m²/kg

Show Supplier Material materials with Film yield of 27.47 - 73.26 m²/kg

Shrinkage

120.0 °C

4 - 5 %

Show Supplier Material materials with Shrinkage of 4 - 5 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Shrinkage, transverse

120.0 °C

2 - 3 %

Show Supplier Material materials with Shrinkage, transverse of 2 - 3 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Surface density

20.0 °C

1.36E-3 - 3.64E-3 g/cm²

Show Supplier Material materials with Surface density of 1.36E-3 - 3.64E-3 g/cm²

Material Information

PropertyValue

Dimension

Available thicknesses: 15, 18, 20, 25, 30, 35, 40µm.

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 - 220 %

Show Supplier Material materials with Elongation of 200 - 220 %

GOST 14236, ISO 527, ASTM D882

Elongation, transverse

20.0 °C

70 - 80 %

Show Supplier Material materials with Elongation, transverse of 70 - 80 %

GOST 14236, ISO 527, ASTM D882

Tensile strength

20.0 °C

130 - 140 MPa

Show Supplier Material materials with Tensile strength of 130 - 140 MPa

GOST 14236, ISO 527, ASTM D882

Tensile strength, transverse

20.0 °C

230 - 250 MPa

Show Supplier Material materials with Tensile strength, transverse of 230 - 250 MPa

GOST 14236, ISO 527, ASTM D882

Technological properties

Property
Application areas

High quality rotogravure and flexographic solvent based printing; for lamination with solvent based or solventless polyurethane adhesives; manufacture of flexible packaging for food products; packaging for vertical VFFS and horizontal HFFS packaging machines; for production of fully wrapped labels for bottles; UT side can be coated by frame cold seal glue.

Friction

Kinetic coefficient of friction µ= 0.15-0.45 (GOST 27492, ISO 8295, ASTM D 1894).

Other

HMPL.M BOPP films comprise: An aluminum layer, a treated modified copolymer layer for aluminum adhesion, a transparent oriented polypropylene core layer, a heat sealable non treated, skin layer with standard coefficient of friction.

Processing history

Treatment level: 36 mN/m (ISO 8296, ASTM D 2578).