Dimension
Property | Value | Comment |
---|---|---|
Diameter | 20 - 800 mm Show Supplier Material materials with Diameter of 20 - 800 mm | |
Length | 2000 - 5800 mm Show Supplier Material materials with Length of 2000 - 5800 mm | |
Thickness | 800 mm Show Supplier Material materials with Thickness of 800 mm | max. |
Width | 205 - 800 mm Show Supplier Material materials with Width of 205 - 800 mm |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 200 - 210 GPa Show Supplier Material materials with Elastic modulus of 200 - 210 GPa at 23.0 °C | 23.0 °C | Typical for Steels |
Hardness, Rockwell C | 64 - 65 [-] Show Supplier Material materials with Hardness, Rockwell C of 64 - 65 [-] at 23.0 °C | 23.0 °C | Quenched |
Chemical properties
Property | ||
---|---|---|
Carbon | 2 - 2.3 % | |
Chromium | 11.5 - 13 % | |
Iron | Balance | |
Manganese | 0.4 % | |
Phosphorus | 0.03 % | |
Silicon | 0.4 % | |
Sulfur | 0.03 % |