1.2379

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Songshun Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValueComment

Diameter

20 - 800 mm

Show Supplier Material materials with Diameter of 20 - 800 mm

Length

300 - 5800 mm

Show Supplier Material materials with Length of 300 - 5800 mm

Thickness

800 mm

Show Supplier Material materials with Thickness of 800 mm

max.

Width

205 - 800 mm

Show Supplier Material materials with Width of 205 - 800 mm

Mechanical

PropertyValueTemperatureComment

Elastic modulus

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa at 23.0 °C

23.0 °C

Typical for Steels

Hardness, Rockwell C

62 - 66 [-]

Show Supplier Material materials with Hardness, Rockwell C of 62 - 66 [-] at 23.0 °C

23.0 °C

Tempered

Chemical properties

Property

Carbon

1.4 - 1.6 %

Chromium

11 - 13 %

Iron

Balance

Manganese

0.6 %

Molybdenum

0.7 - 1.2 %

Phosphorus

0.03 %

Silicon

0.6 %

Sulfur

0.03 %

Vanadium

0.5 - 1.1 %