1.2363

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Songshun Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

50 - 500 mm

Show Supplier Material materials with Diameter of 50 - 500 mm

Length

2000 - 5800 mm

Show Supplier Material materials with Length of 2000 - 5800 mm

Thickness

20 - 400 mm

Show Supplier Material materials with Thickness of 20 - 400 mm

Width

80 - 1000 mm

Show Supplier Material materials with Width of 80 - 1000 mm

Mechanical

PropertyValueTemperatureComment

Elastic modulus

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa at 23.0 °C

23.0 °C

Typical for Steels

Hardness, Brinell

248 [-]

Show Supplier Material materials with Hardness, Brinell of 248 [-] at 23.0 °C

23.0 °C

Annealed

Hardness, Rockwell C

60 - 62 [-]

Show Supplier Material materials with Hardness, Rockwell C of 60 - 62 [-] at 23.0 °C

23.0 °C

Quenched

Chemical properties

Property

Carbon

0.95 - 1.05 %

Chromium

4.75 - 5.5 %

Iron

Balance

Manganese

1 %

Molybdenum

0.9 - 1.4 %

Phosphorus

0.03 %

Silicon

0.5 %

Sulfur

0.03 %

Vanadium

0.15 - 0.5 %