DC03-NiZn Cote electrolytically-plated

Alternative and trade names
nickel zinc alloy electroplated steel, ASTM A109 Grade 1008, EN 10139 Grade DC03, EN 10140 Grade DC03
Want to keep this datasheet? Save it now in your required format

Description

Tata Steel’s NiZn-Cote® and NiZn-Cote® Plus are cold-rolled steel strip products electroplated with a nickel-zinc alloy. These high-performance products provide a cost-effective alternative to stainless steel.


NiZn-Cote® and NiZn-Cote® Plus are successfully used in a wide range of demanding applications. They offer significant benefits for your end-products and processes. These include excellent corrosion resistance and paint adhesion.


Our optimised electroplating process ensures outstanding corrosion resistance. The resistance levels are higher than those of a galvanised coating at equivalent plating thickness.


Main benefits of NiZn-Cote® and NiZn-Cote® Plus include:
  • end-products of consistent and reliable quality
  • improved end-product performance
  • trouble-free, repeatable processing
  • minimised waste
  • opportunities to reduce processing steps
  • opportunities for cost savings
  • control of substrate and base metal properties
  • it can be bent, roll formed, stamped drawn, and coined.


    There are 2 variants of coatings:
  • NiZn-Cote®: electrolytically-plated with a nickel-zinc alloy
  • NiZn-Cote® Plus: electrolytically-plated with a nickel-zinc alloy; with added polymer coating

    Please consult the supplier about other product options.

  • Related Standards

    Equivalent Materials

    This material data has been provided by TATA Steel.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueComment

    Surface roughness

    0 - 2.5 μm

    Show Supplier Material materials with Surface roughness of 0 - 2.5 μm

    depending on the surface finish, please refer to the technological properties Other

    Chemical properties

    PropertyValueComment

    Carbon

    0.1 %

    Show Supplier Material materials with Carbon of 0.1 %

    max.

    Manganese

    0.5 %

    Show Supplier Material materials with Manganese of 0.5 %

    max.

    Phosphorus

    0.04 %

    Show Supplier Material materials with Phosphorus of 0.04 %

    max.

    Sulfur

    0.05 %

    Show Supplier Material materials with Sulfur of 0.05 %

    max.

    Technological properties

    Property
    Application areas

  • Automotive components
  • Electrical components
  • Tubing
  • Brackets
  • Sporting ammunition

  • Other

    Surface roughness (Ra)
    #2 FinishRa: 0.15-0.51 μm (smooth finish)
    #1 FinishRa: 0.6-2.5 μm (rough finish)


    Coil weight
    Strip thickness (mm / inch)max coil weight EU/US
    0.1 – 1.4 / 0.008” – 0.055”10kg/mm coil width (10 KIM) / 700 PIW


    Coil inner diameter (ID)
    mm / inch
    Coil outer diameter (OD)
    mm / inch
    400, 500 / 16”, 20”max. 1368 / 60”


    Coil edge finishes
    Natural edges (#2)strip edges have a mill edge (un-slit edges)
    Slit edges (#3)strip edges have been slit (reduces maximum width by a total of 10mm)
    Straight wound coilsstandard


    Delivery conditionThickness range (mm/inch)Plating thickness (μm/µ")Width range (mm/inch)
    1T (full hard), 2T, 3T, 4T, 5T0.1 - 1.4 / 0.008 - 0.550.5 - 5.0 / 20 - 20012 - 724 / 0.5 - 28.5

    Surface Finish

  • Cold-rolled strip (CRS) smooth to rough finish (KB MA)
  • Natural (as plated)
  • Planished (brushed)