ABS PLUS 3D

Want to keep this datasheet? Save it now in your required format

Description

It is designed for printing in FFF/FDM technology and available in different colors. Increased hardness and durability, high impact resistance, resistance to high temperature and abrasion, possibility of machining and chemical treatment, possibility of printing in open printers

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.1 g/cm³

Show Supplier Material materials with Density of 1.1 g/cm³

ASTM D792

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.02 mm

2.85 mm

Show Supplier Material materials with Diameter of 2.85 mm

Tolerance +/- 0.02 mm

Mechanical

PropertyValueComment

Elongation

30 %

Show Supplier Material materials with Elongation of 30 %

ASTM D638

Flexural modulus

2.15 GPa

Show Supplier Material materials with Flexural modulus of 2.15 GPa

ASTM D790

Flexural strength

60.81 MPa

Show Supplier Material materials with Flexural strength of 60.81 MPa

ASTM D790

Yield strength

37.75 MPa

Show Supplier Material materials with Yield strength of 37.75 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

90 °C

Show Supplier Material materials with Heat deflection temperature of 90 °C

1.8 MPa

ASTM D648, unannealed-annealed condition

100 °C

Show Supplier Material materials with Heat deflection temperature of 100 °C

1.8 MPa

ASTM D648, unannealed-annealed condition

Vicat softening temperature

107.0 °C

Show Supplier Material materials with Vicat softening temperature of 107.0 °C

ASTM D1525

Technological properties

Property
Application areas

END-USE PARTS: containers, holders - PROTOTYPES: mechanical parts, architectural models - ELECTRONICS: covers, cases - DECORATIONS: lamps, vases

Processing methods

Bed heating required, printing temperature: 250-270°C, bed temperature: 90-110°C