Description

It is designed for printing in FFF/FDM technology and available in different colors. Just another option for enthusiast of printing on rubber-like materials. FIBERFLEX 30D is characterized by reduced hardness up to 30D on the Shore scale, very good flexibility and higher impact strength as well as high chemical resistance. The material is recommended especially for printing tires, seals, belts and all kinds of elastic elements.

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.07 g/cm³

Show Supplier Material materials with Density of 1.07 g/cm³

Water absorption

0.8 %

Show Supplier Material materials with Water absorption of 0.8 %

ASTM D570

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.05 mm

Mechanical

PropertyValueComment

Elongation

900 %

Show Supplier Material materials with Elongation of 900 %

ASTM D638

Flexural modulus

0.066 GPa

Show Supplier Material materials with Flexural modulus of 0.066 GPa

ASTM D790

Hardness, Shore D

30.0 [-]

Show Supplier Material materials with Hardness, Shore D of 30.0 [-]

ASTM D2240

Rebound Resilience

72.0 %

Show Supplier Material materials with Rebound Resilience of 72.0 %

ASTM D2632

Tear strength

95.0 kN/m

Show Supplier Material materials with Tear strength of 95.0 kN/m

ASTM D1004

Tensile strength

21.57 MPa

Show Supplier Material materials with Tensile strength of 21.57 MPa

ASTM D638

Thermal

PropertyValueComment

Melting point

174.0 °C

Show Supplier Material materials with Melting point of 174.0 °C

ASTM D3418

Technological properties

Property
Application areas

RUBBER ELEMENTS OF MACHINES: Polymer Gaskets, elements that are frequently bent - GADGETS OR THEIR ELEMENTS: phone sleeves and cases, watch-, pulse counter-, pedometer straps - LINKING ELEMENTS: flexible hinges - TOYS OR THEIR ELEMENTS: tires, rubber figures - JEWELLERY: bands, bracelets

Processing methods

Print temperature: 200 – 220°C, bed temperature: 50 – 70 °C - to remove the print easier, it is recommended to heat the bed to 110°C