Elastic 40D 3D

Want to keep this datasheet? Save it now in your required format

Description

It is designed for printing in FFF/FDM technology and available in different colors, with this flexible material with Shore hardness of D40 you can print at the speed of 45mm/s without worrying about the quality of the print. What’s more, thanks to FIBERFLEX 40D you will discover that printing with flexible filaments doesn’t have to be difficult. Feeding it to the extruder will be extremely easy and the printed layers will stick together well. Your prints will have such properties as: high impact resistance, low temperature resistance, chemical and abrasion resistance. Because of that FIBERFLEX 40D can be used for both amateur and professional applications.

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.16 g/cm³

Show Supplier Material materials with Density of 1.16 g/cm³

Water absorption

0.6 %

Show Supplier Material materials with Water absorption of 0.6 %

ASTM D570

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.05 mm

2.85 mm

Show Supplier Material materials with Diameter of 2.85 mm

Tolerance +/- 0.05 mm

Mechanical

PropertyValueComment

Elongation

680 %

Show Supplier Material materials with Elongation of 680 %

ASTM D638

Flexural modulus

0.066 GPa

Show Supplier Material materials with Flexural modulus of 0.066 GPa

ASTM D790

Hardness, Shore D

40.0 [-]

Show Supplier Material materials with Hardness, Shore D of 40.0 [-]

ASTM D2240

Rebound Resilience

57.0 %

Show Supplier Material materials with Rebound Resilience of 57.0 %

ASTM D2632

Tear strength

115.0 kN/m

Show Supplier Material materials with Tear strength of 115.0 kN/m

ASTM D1004

Tensile strength

26.47 MPa

Show Supplier Material materials with Tensile strength of 26.47 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

70 °C

Show Supplier Material materials with Heat deflection temperature of 70 °C

0.45 MPa

ASTM D648

Melting point

157.0 °C

Show Supplier Material materials with Melting point of 157.0 °C

ASTM D3418

Technological properties

Property
Application areas

RUBBER ELEMENTS OF MACHINES: Polymer Gaskets, elements that are frequently bent - GADGETS OR THEIR ELEMENTS: phone sleeves and cases, watch-, pulse counter-, pedometer straps - LINKING ELEMENTS: flexible hinges - TOYS OR THEIR ELEMENTS: tires, rubber figures - JEWELLERY: bands, bracelets

Processing methods

Print temperature: 200-220°C, bed temperature: 50-70 °C - printing speed up to 45 mm/s with direct extruder, can be printed with Bowden style extruder at speed 15-30 mm/s - to remove the print easier, it is recommended to heat the bed to 110°C