Description

It is designed for printing in FFF/FDM technology and available in different colors, thanks to its resistance to high temperatures, alcohol and chemicals, Nylon is particularly useful for mechanical and technical applications. It is extremely durable, strong and unbreakable. It is easily machined with tools designed for metal processing and it is also easily painted, which makes it even more versatile and functional. It is incredibly flexible – it expands by 50% before it breaks. However, it is not resistant to concentrated alkalis and acids.

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.02 g/cm³

Show Supplier Material materials with Density of 1.02 g/cm³

ISO 483

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.02 mm

Mechanical

PropertyValueComment

Elastic modulus

1.4 GPa

Show Supplier Material materials with Elastic modulus of 1.4 GPa

ISO 527

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

Flexural modulus

1.2 GPa

Show Supplier Material materials with Flexural modulus of 1.2 GPa

ISO 178

Tensile strength

51 MPa

Show Supplier Material materials with Tensile strength of 51 MPa

ISO 527

Thermal

PropertyValueComment

Melting point

180.0 °C

Show Supplier Material materials with Melting point of 180.0 °C

ISO 1133

Rheological Properties

PropertyValueComment

Melt volume-flow rate

180.0 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 180.0 cm³/10min

ISO 11357

Technological properties

Property
Application areas

MECHANICAL PARTS: guides, gears (cog wheels) - TECHNICAL COMPONENTS: slide bearings, nuts

Processing methods

Bed temperature: ca. 100°C, Nozzle temperature: 255-270 °C - No drying required