SY PLA 3D

Want to keep this datasheet? Save it now in your required format

Description

It is designed for printing in FFF/FDM technology and available in different colors. Easy PLA is a material that allows you to achieve prints of a very high quality and avoid complications during the printing process. No matter what level of experience in 3D printing you have,printing with EASY PLA is sure to encourage you to pursue even more ambitious and complex projects. All this thanks to the easiness of printing. But what really matters in the end is the result. Your prints are sure to become something to show off among other 3D printing enthusiasts. After all, not everyone is able to achieve such printing precision. Biodegradability and very good adhesion between the print layers.

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.24 g/cm³

Show Supplier Material materials with Density of 1.24 g/cm³

ASTM D792

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.02 mm

2.85 mm

Show Supplier Material materials with Diameter of 2.85 mm

Tolerance +/- 0.02 mm

Mechanical

PropertyValueComment

Elastic modulus

3.6 GPa

Show Supplier Material materials with Elastic modulus of 3.6 GPa

ASTM D882

Elongation

6 %

Show Supplier Material materials with Elongation of 6 %

ASTM D882

Flexural modulus

3.8 GPa

Show Supplier Material materials with Flexural modulus of 3.8 GPa

ASTM D790

Flexural strength

83 MPa

Show Supplier Material materials with Flexural strength of 83 MPa

ASTM D790

Tensile strength

53 MPa

Show Supplier Material materials with Tensile strength of 53 MPa

ASTM D882

Thermal

PropertyValuePressureComment

Heat deflection temperature

55 °C

Show Supplier Material materials with Heat deflection temperature of 55 °C

0.45 MPa

ASTM E2092

Rheological Properties

PropertyValueComment

Melt mass-flow rate

6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 6 g/10min

ASTM D1238, 210°C/2.16Kg

Technological properties

Property
Application areas

TOYS OR THEIR ELEMENTS: human figures, animals, constructions, houses, vehicles, dice - GADGETS OR THEIR ELEMENTS: key rings, stands, phone cases - PROTOTYPES: new products, concept models - ELEMENTS OF JEWELLERY: earrings, bracelets, beads, necklaces - DECORATIONS: Christmas tree ornaments, pendants

Processing methods

Print temperature: 200-230°C, Bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required), Easy PLA Aurora – recommended minimum 0,5 mm nozzle