Description

It is designed for printing in FFF/FDM technology and available in different colors, this product offers properties that are similar or better than those of ABS filaments while keeping the ease and security of the printing process typical of traditional PLA. This technical filament ensures increased resistance to cracking and breaking due to its high impact strength and a higher resistance to high temperatures. With these properties, it is ideal for creating demanding prints working in extreme conditions while maintaining the highest level of attention to detail. It is a tried and tested filament for printing functional prototypes and large heavy-duty tools. Increased impact strength compared to PLA (up to 800%) and ABS (up to 50%), parameters exceeding the ABS, precise reproduction of details, very good adhesion

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.22 g/cm³

Show Supplier Material materials with Density of 1.22 g/cm³

ASTM D792

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.02 mm

Mechanical

PropertyValueComment

Elastic modulus

2.86 GPa

Show Supplier Material materials with Elastic modulus of 2.86 GPa

ASTM D790

Flexural modulus

2.4 GPa

Show Supplier Material materials with Flexural modulus of 2.4 GPa

ASTM D790

Flexural strength

73 MPa

Show Supplier Material materials with Flexural strength of 73 MPa

ASTM D790

Tensile strength

40 MPa

Show Supplier Material materials with Tensile strength of 40 MPa

ASTM D638

Thermal

PropertyValuePressure

Heat deflection temperature

75 °C

Show Supplier Material materials with Heat deflection temperature of 75 °C

0.45 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature of 85 °C

0.45 MPa

Rheological Properties

PropertyValueComment

Melt mass-flow rate

9 g/10min

Show Supplier Material materials with Melt mass-flow rate of 9 g/10min

ASTM D1238 , 210°C/2.16Kg

15 g/10min

Show Supplier Material materials with Melt mass-flow rate of 15 g/10min

ASTM D1238 , 210°C/2.16Kg

Technological properties

Property
Application areas

TOYS OR THEIR ELEMENTS: blocks, works or parts thereof, car parts - PROTOTYPES: tools, conceptual models, switching parts, mechanical parts, elements requiring resistance to higher temperatures - SPARE PARTS: elements of machines, devices, vehicles, electronic equipment - TOOLS OR THEIR ELEMENTS: gears, racks, elements requiring high strength - READY PRODUCTS: containers, handles - TOYS OR THEIR ELEMENTS: blocks, robots or their parts, car parts

Processing methods

Print temperature 220-245°C, Bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required)