Description

It is designed for printing in FFF/FDM technology and available in different colors. It is a material that resembles plaster casting. This distinctive feature, combined with the precision of the prints, makes it possible to use it in architectural and artistic studios, detailed prototyping and modelling. No shape poses a challenge for this product. Its properties allow for accurate replication of even the tiniest elements.

This material data has been provided by Advanced Manufacturing Technologies.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.4 g/cm³

Show Supplier Material materials with Density of 1.4 g/cm³

Dimension

PropertyValueComment

Diameter

1.75 mm

Show Supplier Material materials with Diameter of 1.75 mm

Tolerance +/- 0.02 mm

2.85 mm

Show Supplier Material materials with Diameter of 2.85 mm

Tolerance +/- 0.02 mm

Mechanical

PropertyValue

Elastic modulus

3.5 GPa

Show Supplier Material materials with Elastic modulus of 3.5 GPa

Elongation at yield

3.2 %

Show Supplier Material materials with Elongation at yield of 3.2 %

Tensile strength

43 MPa

Show Supplier Material materials with Tensile strength of 43 MPa

Thermal

PropertyValuePressure

Heat deflection temperature

48 °C

Show Supplier Material materials with Heat deflection temperature of 48 °C

0.45 MPa

Rheological Properties

PropertyValueComment

Melt volume-flow rate

16.0 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 16.0 cm³/10min

190°C/2.16Kg

Technological properties

Property
Application areas

MODELS: buildings, structures, land development projects, interiors - DECORATIONS: statues, sculptures, reliefs - MODELING: small elements requiring high precision - PROTOTYPES: concept models, small parts

Processing methods

Print temperature: 190-210°C, Bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required)