Cp-Ti Gr 1 (Size cuts: -53µm/+20µm)

Want to keep this datasheet? Save it now in your required format

Description

Pure Titanium that indicates the following properties:


  • Excellent flowability
  • Plasma atomized, highly spherical
  • High packing density
  • Low porosity
  • Little to no sattelites and high chemical purity
  • This material data has been provided by Advanced Manufacturing Technologies.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValue

    Bulk density

    2.47 - 2.56 g/cm³

    Show Supplier Material materials with Bulk density of 2.47 - 2.56 g/cm³

    Particle size D10

    26.0 - 31.0 μm

    Show Supplier Material materials with Particle size D10 of 26.0 - 31.0 μm

    Particle size D50

    38.0 - 43.0 μm

    Show Supplier Material materials with Particle size D50 of 38.0 - 43.0 μm

    Particle size D90

    50.0 - 55.0 μm

    Show Supplier Material materials with Particle size D90 of 50.0 - 55.0 μm

    Rheological Properties

    PropertyValue

    Hall flow

    28 s/50g

    Show Supplier Material materials with Hall flow of 28 s/50g

    32 s/50g

    Show Supplier Material materials with Hall flow of 32 s/50g

    Chemical properties

    PropertyValueComment

    Carbon

    0.08 %

    Show Supplier Material materials with Carbon of 0.08 %

    Maximum

    Hydrogen

    0.015 %

    Show Supplier Material materials with Hydrogen of 0.015 %

    Iron

    0.2 %

    Show Supplier Material materials with Iron of 0.2 %

    Nitrogen

    0.03 %

    Show Supplier Material materials with Nitrogen of 0.03 %

    Other

    0.4 %

    Show Supplier Material materials with Other of 0.4 %

    Total Maximum

    Oxygen

    0.18 %

    Show Supplier Material materials with Oxygen of 0.18 %

    Titanium

    Balance

    Technological properties

    Property
    Application areas

    Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace