Inconel 718 powder (Size cuts: -90µm/+45µm)

Want to keep this datasheet? Save it now in your required format

Description

Nickel Iron Alloy that indicates the following properties:


  • Excellent flowability
  • Plasma atomized, highly spherical
  • High packing density
  • Low porosity
  • Few sattelites and high chemical purity
  • This material data has been provided by Advanced Manufacturing Technologies.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValue

    Bulk density

    4.65 - 4.8 g/cm³

    Show Supplier Material materials with Bulk density of 4.65 - 4.8 g/cm³

    Particle size D10

    42.0 - 46.0 μm

    Show Supplier Material materials with Particle size D10 of 42.0 - 46.0 μm

    Particle size D50

    60.0 - 65.0 μm

    Show Supplier Material materials with Particle size D50 of 60.0 - 65.0 μm

    Particle size D90

    85.0 - 90.0 μm

    Show Supplier Material materials with Particle size D90 of 85.0 - 90.0 μm

    Rheological Properties

    PropertyValue

    Hall flow

    12 s/50g

    Show Supplier Material materials with Hall flow of 12 s/50g

    14 s/50g

    Show Supplier Material materials with Hall flow of 14 s/50g

    Chemical properties

    PropertyValueComment

    Aluminium

    0.61 %

    Show Supplier Material materials with Aluminium of 0.61 %

    Boron

    0.005 %

    Show Supplier Material materials with Boron of 0.005 %

    Maximum

    Carbon

    0.02 %

    Show Supplier Material materials with Carbon of 0.02 %

    Chromium

    17.6 %

    Show Supplier Material materials with Chromium of 17.6 %

    Cobalt

    0.17 %

    Show Supplier Material materials with Cobalt of 0.17 %

    Copper

    0.04 %

    Show Supplier Material materials with Copper of 0.04 %

    Hydrogen

    0.0004 %

    Show Supplier Material materials with Hydrogen of 0.0004 %

    Iron

    18.5 %

    Show Supplier Material materials with Iron of 18.5 %

    Manganese

    0.07 %

    Show Supplier Material materials with Manganese of 0.07 %

    Molybdenum

    2.89 %

    Show Supplier Material materials with Molybdenum of 2.89 %

    Nickel

    54.17 %

    Show Supplier Material materials with Nickel of 54.17 %

    Niobium

    5.14 %

    Show Supplier Material materials with Niobium of 5.14 %

    Nitrogen

    0.01 %

    Show Supplier Material materials with Nitrogen of 0.01 %

    Oxygen

    0.01 %

    Show Supplier Material materials with Oxygen of 0.01 %

    Phosphorus

    0.005 %

    Show Supplier Material materials with Phosphorus of 0.005 %

    Silicon

    0.07 %

    Show Supplier Material materials with Silicon of 0.07 %

    Sulfur

    0.001 %

    Show Supplier Material materials with Sulfur of 0.001 %

    Maximum

    Titanium

    0.97 %

    Show Supplier Material materials with Titanium of 0.97 %

    Tungsten

    0.03 %

    Show Supplier Material materials with Tungsten of 0.03 %

    Vanadium

    0.04 %

    Show Supplier Material materials with Vanadium of 0.04 %

    Technological properties

    Property
    Application areas

    Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace