UGI® 4105 Annealed

Want to keep this datasheet? Save it now in your required format

Description

Screw machining stainless steel with 17% chromium used in relatively unaggressive environments and which can be optimized by UGIMA® process without impairing its mechanical and corrosion resistance properties.

Related Standards

Equivalent Materials

This material data has been provided by Ugitech SA.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyValueComment

Elongation

7.0 - 20.0 %

Show Supplier Material materials with Elongation of 7.0 - 20.0 %

min., depending on the size

Tensile strength

430.0 - 780.0 MPa

Show Supplier Material materials with Tensile strength of 430.0 - 780.0 MPa

depending on the size

Chemical properties

PropertyValueComment

Carbon

0.08

Show Supplier Material materials with Carbon of 0.08

max.

Chromium

17.0 %

Show Supplier Material materials with Chromium of 17.0 %

Sulfur

0.25 %

Show Supplier Material materials with Sulfur of 0.25 %

Technological properties

Property
Application areas

Transport, electronic equipment, food and food processing industry, decoration, household appliances and office systems. Machined parts, screw machining.

Corrosion properties

Approximately the same as for ferritic stainless steels with 17% chromium of the AISI 430 type, although its corrosion resistance is adversely affected by its high sulphur content, particularly in environments conducive to pitting or crevice corrosion.

Other

Available products:


ProductShapeFinishingToleranceDimensions (mm)


Bar


Round
Rolled descaledk13Ø 22 to 70
Turned10+11Ø 22 to 70
Ground7+8+9+optionsØ 2 to 70
Drawn9 Ø 2 to 30
Black bar±1% of ∅Ø 23 to 73
BilletSquare50 to 120


Other products: contact the supplier