UGI® 4763 Cold Drawn

Want to keep this datasheet? Save it now in your required format

Description

Ferritic steel with a high chromium content used in high temperature applications from 800°C to 1100°C, offering good resistance to cyclic oxidation. Good ferromagnetic properties.

Related Standards

Equivalent Materials

This material data has been provided by Ugitech SA.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyValueComment

Elongation

10.0 - 15.0 %

Show Supplier Material materials with Elongation of 10.0 - 15.0 %

min., depending on the size

Tensile strength

450.0 - 750.0 MPa

Show Supplier Material materials with Tensile strength of 450.0 - 750.0 MPa

depending on the size

Chemical properties

PropertyValueComment

Carbon

0.05

Show Supplier Material materials with Carbon of 0.05

max.

Chromium

24.0 %

Show Supplier Material materials with Chromium of 24.0 %

Nitrogen

0.05 %

Show Supplier Material materials with Nitrogen of 0.05 %

Technological properties

Property
Application areas

Parts and accessories for heat treatment furnace and quenching baths. Solenoid valve components.

Other

Available products:


ProductShapeFinishingToleranceDimensions (mm)
BarRoundRolled descaledk13Ø 22 to 70
Turned10+11Ø 22 to 70
Ground7+8+9+optionsØ 2 to 70
Drawn9 Ø 2 to 30
Black bar±1% of ∅Ø 23 to 73
BilletSquare50 to 120


Other products: contact the supplier