ASTM B387 Grade Type 366

Want to keep this datasheet? Save it now in your required format

Description

Melt metallurgical molybdenum-tungsten (MoW).

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

10.2 g/cm³

Show Material materials with Density of 10.2 g/cm³

Typical for Molybdenum

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

324 GPa

Show Material materials with Elastic modulus of 324 GPa

Typical for Molybdenum

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Molybdenum

Shear modulus

23.0 °C

125 GPa

Show Material materials with Shear modulus of 125 GPa

Typical for Molybdenum

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

4E-6 - 1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 4E-6 - 1.4E-5 1/K

Typical for Molybdenum

Melting point

2610 °C

Show Material materials with Melting point of 2610 °C

Typical for Molybdenum

Specific heat capacity

23.0 °C

201 - 280 J/(kg·K)

Show Material materials with Specific heat capacity of 201 - 280 J/(kg·K)

Typical for Molybdenum

Thermal conductivity

23.0 °C

117 - 431 W/(m·K)

Show Material materials with Thermal conductivity of 117 - 431 W/(m·K)

Typical for Molybdenum

Chemical properties

PropertyValue

Carbon

0.03 %

Show Material materials with Carbon of 0.03 %

Iron

0.01 %

Show Material materials with Iron of 0.01 %

Nickel

2E-3 %

Show Material materials with Nickel of 2E-3 %

Nitrogen

2E-3 %

Show Material materials with Nitrogen of 2E-3 %

Oxygen

2.5E-3 %

Show Material materials with Oxygen of 2.5E-3 %

Silicon

0.01 %

Show Material materials with Silicon of 0.01 %

Tungsten

27 - 33 %

Show Material materials with Tungsten of 27 - 33 %