General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 6.55 g/cm³ Show Material materials with Density of 6.55 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 68 GPa Show Material materials with Elastic modulus of 68 GPa | Typical for Zirconium |
Elongation A50 | 20.0 °C | 15 % Show Material materials with Elongation A50 of 15 % | |
Elongation A50, transverse | 20.0 °C | 15 % Show Material materials with Elongation A50, transverse of 15 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Zirconium |
Shear modulus | 23.0 °C | 35 GPa Show Material materials with Shear modulus of 35 GPa | Typical for Zirconium |
Tensile strength | 20.0 °C | 510 MPa Show Material materials with Tensile strength of 510 MPa | |
Tensile strength, transverse | 20.0 °C | 510 MPa Show Material materials with Tensile strength, transverse of 510 MPa | |
Yield strength Rp0.2 | 20.0 °C | 345 MPa Show Material materials with Yield strength Rp0.2 of 345 MPa | |
Yield strength Rp0.2, transverse | 20.0 °C | 385 MPa Show Material materials with Yield strength Rp0.2, transverse of 385 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.7E-6 - 7E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.7E-6 - 7E-6 1/K | Typical for Zirconium |
Melting point | 1845 °C Show Material materials with Melting point of 1845 °C | Typical for Zirconium | |
Specific heat capacity | 23.0 °C | 281 - 289 J/(kg·K) Show Material materials with Specific heat capacity of 281 - 289 J/(kg·K) | Typical for Zirconium |
Thermal conductivity | 23.0 °C | 19 - 27 W/(m·K) Show Material materials with Thermal conductivity of 19 - 27 W/(m·K) | Typical for Zirconium |
Chemical properties
Property | Value |
---|---|
Niobium | 2.4 - 2.8 % Show Material materials with Niobium of 2.4 - 2.8 % |
Oxygen | 0.09 - 0.15 % Show Material materials with Oxygen of 0.09 - 0.15 % |