General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.57 g/cm³ Show Material materials with Density of 8.57 g/cm³ | Typical for Niobium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 104 GPa Show Material materials with Elastic modulus of 104 GPa | Typical for Niobium |
Hardness, Brinell | 20.0 °C | 135 - 150 [-] Show Material materials with Hardness, Brinell of 135 - 150 [-] | |
Poisson's ratio | 23.0 °C | 0.4 [-] Show Material materials with Poisson's ratio of 0.4 [-] | Typical for Niobium |
Shear modulus | 23.0 °C | 38 GPa Show Material materials with Shear modulus of 38 GPa | Typical for Niobium |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 6.8E-6 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 6.8E-6 - 1.4E-5 1/K | Typical for Niobium |
Melting point | 2468 °C Show Material materials with Melting point of 2468 °C | Typical for Niobium | |
Specific heat capacity | 23.0 °C | 201 - 272 J/(kg·K) Show Material materials with Specific heat capacity of 201 - 272 J/(kg·K) | Typical for Niobium |
Thermal conductivity | 23.0 °C | 53 - 54 W/(m·K) Show Material materials with Thermal conductivity of 53 - 54 W/(m·K) | Typical for Niobium |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Carbon | 0.01 % Show Material materials with Carbon of 0.01 % |
Hafnium | 0.02 % Show Material materials with Hafnium of 0.02 % |
Hydrogen | 1.5E-3 % Show Material materials with Hydrogen of 1.5E-3 % |
Iron | 0.01 % Show Material materials with Iron of 0.01 % |
Molybdenum | 0.05 % Show Material materials with Molybdenum of 0.05 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Nitrogen | 0.01 % Show Material materials with Nitrogen of 0.01 % |
Oxygen | 0.03 % Show Material materials with Oxygen of 0.03 % |
Silicon | 5E-3 % Show Material materials with Silicon of 5E-3 % |
Tantalum | 0.5 % Show Material materials with Tantalum of 0.5 % |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % |
Tungsten | 0.05 % Show Material materials with Tungsten of 0.05 % |
Zirconium | 0.8 - 1.2 % Show Material materials with Zirconium of 0.8 - 1.2 % |