Reactor grade niobium-zirconium alloy seamles and welded tubes.
See where ASTM B394 Grade R04251 soft annealed (+A) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.57 g/cm³ at 20 °C
Thermal conductivity
λ52 W/(m·K) at 20 °C
Electrical resistivity
ρel1.5E-7 Ω·m at 20 °C
Element
Weight %
Comment
0.8 - 1.2 %
0.1 %
0.03 %
0.02 %
0.02 %
This material data has been provided by WIAM.