ASTM B394 Grade R04261 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

Commercial grade niobium-zirconium alloy seamless and welded tubes.

Related Standards

Ashby charts

See where ASTM B394 Grade R04261 soft annealed (+A) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.57 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

103 GPa at 20 °C

Show Niobium materials with Elastic modulus of 103 GPa at 20 °C

Elongation A25

A25

20 % at 20 °C

Show Niobium materials with Elongation A25 of 20 % at 20 °C

Tensile strength

Rm

195 MPa at 20 °C

Show Niobium materials with Tensile strength of 195 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

125 MPa at 20 °C

Show Niobium materials with Yield strength Rp0.2 of 125 MPa at 20 °C

Thermal

Thermal conductivity

λ

52 W/(m·K) at 20 °C

Hide chart

Electrical

Electrical resistivity

ρel

1.5E-7 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Zr

0.8 - 1.2 %

Ta

0.5 %

Mo

0.05 %

W

0.05 %

Ti

0.03 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.