Zirconium-niobium alloy forging.
See where ASTM B493 Grade R60705 soft annealed (+A) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ6.64 g/cm³ at 20 °C
Coefficient of thermal expansion
α5.7E-6 - 7E-6 1/K at 23 °C
Typical for Zirconium
Melting point
Tm1845 °C
Typical for Zirconium
Specific heat capacity
cp280.5 J/(kg·K) at 100 °C
Thermal conductivity
λ17.1 W/(m·K) at 20 °C
Element
Weight %
Comment
4.5 %
2 - 3 %
0.18 %
0.05 %
0.03 %
This material data has been provided by WIAM.