Seamless and welded tantalum-columbium alloy tubes with excellent corrosion resistance.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

16.4 g/cm³

Show Material materials with Density of 16.4 g/cm³

Typical for Tantalum

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

185 GPa

Show Material materials with Elastic modulus of 185 GPa

Typical for Tantalum

Elongation A25

20.0 °C

20 %

Show Material materials with Elongation A25 of 20 %

Elongation A50

20.0 °C

20 %

Show Material materials with Elongation A50 of 20 %

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Tantalum

Shear modulus

23.0 °C

69 GPa

Show Material materials with Shear modulus of 69 GPa

Typical for Tantalum

Tensile strength

20.0 °C

226 MPa

Show Material materials with Tensile strength of 226 MPa

Yield strength Rp0.2

20.0 °C

193 MPa

Show Material materials with Yield strength Rp0.2 of 193 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.5E-6 1/K

Typical for Tantalum

Melting point

2996 °C

Show Material materials with Melting point of 2996 °C

Typical for Tantalum

Specific heat capacity

23.0 °C

147 J/(kg·K)

Show Material materials with Specific heat capacity of 147 J/(kg·K)

Typical for Tantalum

Thermal conductivity

23.0 °C

52 - 57 W/(m·K)

Show Material materials with Thermal conductivity of 52 - 57 W/(m·K)

Typical for Tantalum

Chemical properties

PropertyValue

Carbon

0.01 %

Show Material materials with Carbon of 0.01 %

Hydrogen

1.5E-3 %

Show Material materials with Hydrogen of 1.5E-3 %

Iron

0.01 %

Show Material materials with Iron of 0.01 %

Molybdenum

0.02 %

Show Material materials with Molybdenum of 0.02 %

Nickel

0.01 %

Show Material materials with Nickel of 0.01 %

Niobium

35 - 42 %

Show Material materials with Niobium of 35 - 42 %

Nitrogen

0.01 %

Show Material materials with Nitrogen of 0.01 %

Oxygen

0.02 %

Show Material materials with Oxygen of 0.02 %

Silicon

5E-3 %

Show Material materials with Silicon of 5E-3 %

Titanium

0.01 %

Show Material materials with Titanium of 0.01 %

Tungsten

0.05 %