Seamless and welded tubes from unalloyed zirconium.
See where ASTM B523 Grade R60702 soft annealed (+A) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ6.51 g/cm³ at 20 °C
Coefficient of thermal expansion
α5.7E-6 - 7E-6 1/K at 23 °C
Typical for Zirconium
Melting point
Tm1845 °C
Typical for Zirconium
Specific heat capacity
cp284.7 J/(kg·K) at 100 °C
Thermal conductivity
λ22 W/(m·K) at 20 °C
Element
Weight %
Comment
4.5 %
0.16 %
0.05 %
0.03 %
5E-3 %
This material data has been provided by WIAM.