ASTM B523 Grade R60704 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

Seamless and welded tubes from zirconium-tin alloy.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

6.57 g/cm³

Show Material materials with Density of 6.57 g/cm³

Typical for Zirconium

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

68 GPa

Show Material materials with Elastic modulus of 68 GPa

Typical for Zirconium

Elongation A50

20.0 °C

14 %

Show Material materials with Elongation A50 of 14 %

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Zirconium

Shear modulus

23.0 °C

35 GPa

Show Material materials with Shear modulus of 35 GPa

Typical for Zirconium

Tensile strength

20.0 °C

415 MPa

Show Material materials with Tensile strength of 415 MPa

Yield strength Rp0.2

20.0 °C

240 MPa

Show Material materials with Yield strength Rp0.2 of 240 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5.7E-6 - 7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.7E-6 - 7E-6 1/K

Typical for Zirconium

Melting point

1845 °C

Show Material materials with Melting point of 1845 °C

Typical for Zirconium

Specific heat capacity

23.0 °C

281 - 289 J/(kg·K)

Show Material materials with Specific heat capacity of 281 - 289 J/(kg·K)

Typical for Zirconium

Thermal conductivity

23.0 °C

19 - 27 W/(m·K)

Show Material materials with Thermal conductivity of 19 - 27 W/(m·K)

Typical for Zirconium

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Hafnium

4.5 %

Show Material materials with Hafnium of 4.5 %

Hydrogen

5E-3 %

Show Material materials with Hydrogen of 5E-3 %

Nitrogen

0.03 %

Show Material materials with Nitrogen of 0.03 %

Oxygen

0.18 %

Show Material materials with Oxygen of 0.18 %

Tin

1 - 2 %

Show Material materials with Tin of 1 - 2 %