General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 6.57 g/cm³ Show Material materials with Density of 6.57 g/cm³ | Typical for Zirconium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 68 GPa Show Material materials with Elastic modulus of 68 GPa | Typical for Zirconium |
Elongation A50 | 20.0 °C | 12 % Show Material materials with Elongation A50 of 12 % | |
Hardness, Brinell | 20.0 °C | 235 [-] Show Material materials with Hardness, Brinell of 235 [-] | |
Hardness, Rockwell B | 20.0 °C | 99 [-] Show Material materials with Hardness, Rockwell B of 99 [-] | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Zirconium |
Shear modulus | 23.0 °C | 35 GPa Show Material materials with Shear modulus of 35 GPa | Typical for Zirconium |
Tensile strength | 20.0 °C | 483 MPa Show Material materials with Tensile strength of 483 MPa | |
Yield strength Rp0.2 | 20.0 °C | 345 MPa Show Material materials with Yield strength Rp0.2 of 345 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.7E-6 - 7E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.7E-6 - 7E-6 1/K | Typical for Zirconium |
Melting point | 1845 °C Show Material materials with Melting point of 1845 °C | Typical for Zirconium | |
Specific heat capacity | 23.0 °C | 281 - 289 J/(kg·K) Show Material materials with Specific heat capacity of 281 - 289 J/(kg·K) | Typical for Zirconium |
Thermal conductivity | 23.0 °C | 19 - 27 W/(m·K) Show Material materials with Thermal conductivity of 19 - 27 W/(m·K) | Typical for Zirconium |
Chemical properties
Property | Value |
---|---|
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % |
Hafnium | 4.5 % Show Material materials with Hafnium of 4.5 % |
Hydrogen | 5E-3 % Show Material materials with Hydrogen of 5E-3 % |
Niobium | 2 - 3 % Show Material materials with Niobium of 2 - 3 % |
Nitrogen | 0.03 % Show Material materials with Nitrogen of 0.03 % |
Oxygen | 0.3 % Show Material materials with Oxygen of 0.3 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |