Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 20 % Show Material materials with Elongation A50 of 20 % |
316.0 °C | 25 % Show Material materials with Elongation A50 of 25 % | |
Elongation A50, transverse | 20.0 °C | 20 % Show Material materials with Elongation A50, transverse of 20 % |
316.0 °C | 30 % Show Material materials with Elongation A50, transverse of 30 % | |
Tensile strength | 20.0 °C | 400 MPa Show Material materials with Tensile strength of 400 MPa |
316.0 °C | 172 MPa Show Material materials with Tensile strength of 172 MPa | |
Tensile strength, transverse | 20.0 °C | 310 MPa Show Material materials with Tensile strength, transverse of 310 MPa |
316.0 °C | 158 MPa Show Material materials with Tensile strength, transverse of 158 MPa | |
Yield strength Rp0.2 | 20.0 °C | 151 MPa Show Material materials with Yield strength Rp0.2 of 151 MPa |
316.0 °C | 76 MPa Show Material materials with Yield strength Rp0.2 of 76 MPa | |
Yield strength Rp0.2, transverse | 20.0 °C | 172 MPa Show Material materials with Yield strength Rp0.2, transverse of 172 MPa |
316.0 °C | 96 MPa Show Material materials with Yield strength Rp0.2, transverse of 96 MPa | |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Carbon | 0.015 % Show Material materials with Carbon of 0.015 % |
Chromium | 0.01 % Show Material materials with Chromium of 0.01 % |
Copper | 0.01 % Show Material materials with Copper of 0.01 % |
Hydrogen | 2.5E-3 % Show Material materials with Hydrogen of 2.5E-3 % |
Iron | 0.05 % Show Material materials with Iron of 0.05 % |
Molybdenum | 2E-3 % Show Material materials with Molybdenum of 2E-3 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Niobium | 0.01 % Show Material materials with Niobium of 0.01 % |
Nitrogen | 0.01 % Show Material materials with Nitrogen of 0.01 % |
Oxygen | 0.04 % Show Material materials with Oxygen of 0.04 % |
Silicon | 0.01 % Show Material materials with Silicon of 0.01 % |
Tantalum | 0.02 % Show Material materials with Tantalum of 0.02 % |
Tin | 5E-3 % Show Material materials with Tin of 5E-3 % |
Titanium | 0.01 % Show Material materials with Titanium of 0.01 % |
Tungsten | 0.02 % Show Material materials with Tungsten of 0.02 % |
Uranium | 1E-3 % Show Material materials with Uranium of 1E-3 % |
Vanadium | 5E-3 % Show Material materials with Vanadium of 5E-3 % |