General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.57 g/cm³ Show Material materials with Density of 8.57 g/cm³ | Typical for Niobium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 104 GPa Show Material materials with Elastic modulus of 104 GPa | Typical for Niobium |
Elongation A25 | 20.0 °C | 20 % Show Material materials with Elongation A25 of 20 % | |
1100.0 °C | 20 % Show Material materials with Elongation A25 of 20 % | ||
Poisson's ratio | 23.0 °C | 0.4 [-] Show Material materials with Poisson's ratio of 0.4 [-] | Typical for Niobium |
Shear modulus | 23.0 °C | 38 GPa Show Material materials with Shear modulus of 38 GPa | Typical for Niobium |
Tensile strength | 20.0 °C | 370 - 385 MPa Show Material materials with Tensile strength of 370 - 385 MPa | |
1100.0 °C | 145 MPa Show Material materials with Tensile strength of 145 MPa | ||
Yield strength Rp0.2 | 20.0 °C | 260 - 275 MPa Show Material materials with Yield strength Rp0.2 of 260 - 275 MPa | |
1100.0 °C | 110 MPa Show Material materials with Yield strength Rp0.2 of 110 MPa | ||
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 6.8E-6 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 6.8E-6 - 1.4E-5 1/K | Typical for Niobium |
Melting point | 2468 °C Show Material materials with Melting point of 2468 °C | Typical for Niobium | |
Specific heat capacity | 23.0 °C | 201 - 272 J/(kg·K) Show Material materials with Specific heat capacity of 201 - 272 J/(kg·K) | Typical for Niobium |
Thermal conductivity | 23.0 °C | 53 - 54 W/(m·K) Show Material materials with Thermal conductivity of 53 - 54 W/(m·K) | Typical for Niobium |
Chemical properties
Property | Value |
---|---|
Carbon | 0.015 % Show Material materials with Carbon of 0.015 % |
Hafnium | 9 - 11 % Show Material materials with Hafnium of 9 - 11 % |
Hydrogen | 1.5E-3 % Show Material materials with Hydrogen of 1.5E-3 % |
Nitrogen | 0.01 % Show Material materials with Nitrogen of 0.01 % |
Oxygen | 0.03 % Show Material materials with Oxygen of 0.03 % |
Tantalum | 0.5 % Show Material materials with Tantalum of 0.5 % |
Titanium | 0.7 - 1.3 % Show Material materials with Titanium of 0.7 - 1.3 % |
Tungsten | 0.5 % Show Material materials with Tungsten of 0.5 % |
Zirconium | 0.7 % Show Material materials with Zirconium of 0.7 % |