Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 190 GPa Show Material materials with Elastic modulus of 190 GPa |
100.0 °C | 187 GPa Show Material materials with Elastic modulus of 187 GPa | |
150.0 °C | 185 GPa Show Material materials with Elastic modulus of 185 GPa | |
200.0 °C | 183 GPa Show Material materials with Elastic modulus of 183 GPa | |
230.0 °C | 182 GPa Show Material materials with Elastic modulus of 182 GPa | |
Hardness, Vickers | 20.0 °C | 150 [-] Show Material materials with Hardness, Vickers of 150 [-] |
Chemical properties
Property | Value |
---|---|
Carbon | 3E-3 - 5E-3 % Show Material materials with Carbon of 3E-3 - 5E-3 % |
Hydrogen | 5E-4 - 1E-3 % Show Material materials with Hydrogen of 5E-4 - 1E-3 % |
Iron | 0.01 % Show Material materials with Iron of 0.01 % |
Molybdenum | 0.01 - 0.02 % Show Material materials with Molybdenum of 0.01 - 0.02 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Niobium | 0.04 - 0.1 % Show Material materials with Niobium of 0.04 - 0.1 % |
Nitrogen | 3E-3 - 5E-3 % Show Material materials with Nitrogen of 3E-3 - 5E-3 % |
Silicon | 2.5E-3 - 5E-3 % Show Material materials with Silicon of 2.5E-3 - 5E-3 % |
Titanium | 4E-3 - 5E-3 % Show Material materials with Titanium of 4E-3 - 5E-3 % |
Tungsten | 2.2 - 3.5 % Show Material materials with Tungsten of 2.2 - 3.5 % |