Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Chromium Steel
ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type E Class 4 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A387 Grade 12 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type A Class 2 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type D Class 1 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type A Class 1 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type B Class 1 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4140 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von: