Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10216-2 Grade St 45.8 normalized or normalized formed (+N)Martensitischer Edelstahl
DIN 17440 Grade X12Cr13 soft annealed (+A)Ferritischer Edelstahl
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10088-1 Grade X6Cr13 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT)Ferritischer Edelstahl
EN 10088-1 Grade X2CrTi17 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X6Cr13 soft annealed (+A)Ferritischer Edelstahl
EN 10028-7 Grade X2CrNi12 soft annealed (+A)Ferritischer Edelstahl
EN 10028-7 Grade X2CrTi17 soft annealed (+A)Molybdenum Steel
EN 10216-2 Grade 16Mo3 normalized or normalized formed (+N)Molybdenum Steel
EN 10217-2 Grade 16Mo3 normalized or normalized formed (+N)Molybdenum Steel
EN 10217-5 Grade 16Mo3 normalized or normalized formed (+N)Ferritischer Edelstahl
EN 10088-4 Grade X2CrTi12 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT2)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT1)Ferritischer Edelstahl
EN 10088-1 Grade X2CrNi12 quenched and tempered (+QT)Martensitischer Edelstahl
DIN 17440 Grade X10Cr13 quenched and tempered (+QT)Ferritischer Edelstahl
DIN 17441 Grade X6CrTi12 soft annealed (+A)Molybdenum Steel
DIN 17155 Grade 15Mo3 normalized or normalized formed (+N)