Polyamide 6T (PA6T)
Zytel® HTNLTFR52G30NH BL662Polybutylenterephthalat (PBT)
Polybutylene terephthalate Reinforced with 30% Glass Fibre (PBT+GF30)Geliefert von:
4 Matmatch-Lieferanten
Polyetheretherketon (PEEK)
Polyetheretherketone Reinforced with 30% Glass Fibre (PEEK+GF30)Geliefert von:
1 Matmatch-Lieferant
Polyamide 6 (PA6)
Polyamide 6 Reinforced with 50% Glass Fibers (PA6+GF50)Geliefert von:
2 Matmatch-Lieferanten
Polyethylenterephthalat (PET)
Polyethylene terephthalate Reinforced with 30% Glass Fibre (PET+GF30)Geliefert von:
1 Matmatch-Lieferant
Polyamide 66 (PA66)
Polyamide 66 Reinforced with 30% Long Glass Fibers (PA66+LGF30)Geliefert von:
3 Matmatch-Lieferanten
Polyamide 46 (PA46)
Polyamide 46 Reinforced with 50% Glass Fibers (PA46+GF50)Geliefert von:
2 Matmatch-Lieferanten
Polyethersulfon (PES)
Polyethersulfone Reinforced with 30% Glass Fibre (PES+GF30)Styrol-Acrylnitril (SAN)
Styrene acrylonitrile Reinforced with 35% Glass Fibre (SAN+GF35)Polyamide 46 (PA46)
Polyamide 46 Reinforced with 40% Glass Fibers (PA46+GF40)Geliefert von:
1 Matmatch-Lieferant