Polyamide 66 Reinforced with 30% Long Glass Fibers (PA66+LGF30)

Alternative and trade names
Radistrong®, Celstran®, Novamid®, Akulon®,Radistrong®, Radilon®, Radiflam®
Want to keep this datasheet? Save it now in your required format

Description

Polyamide 66 (PA66) with 30% long glass fiber reinforced injection moulding grade, Heat stabilized. Suitable for structural and metal replacement applications, where high stiffness and mechanical resistance are required. Superior impact resistance. Very good heat ageing properties retention.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.35 - 1.37 g/cm³

Show Material materials with Density of 1.35 - 1.37 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

7.0 - 13.0 GPa

Show Material materials with Elastic modulus of 7.0 - 13.0 GPa

Elongation

2.0 - 4.0 %

Show Material materials with Elongation of 2.0 - 4.0 %

Impact strength, Charpy notched

20.0 - 35.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 20.0 - 35.0 kJ/m²

Impact strength, Charpy unnotched

65 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 65 kJ/m²

90 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

Tensile strength

155.0 - 190.0 MPa

Show Material materials with Tensile strength of 155.0 - 190.0 MPa

at 2-4% strain

Thermal

PropertyValue

Melting point

260 °C

Show Material materials with Melting point of 260 °C

Specific heat capacity

1400.0 - 1500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1400.0 - 1500.0 J/(kg·K)

Thermal conductivity

0.27 - 0.33 W/(m·K)

Show Material materials with Thermal conductivity of 0.27 - 0.33 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Electrical resistivity

10000000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Electronic components, lightweight replacement for metals, housings

Fillers

30% Long Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, compression molding