General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.43 g/cm³ Show Supplier Material materials with Density of 1.43 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Water absorption | 5.1 % Show Supplier Material materials with Water absorption of 5.1 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 10.8 GPa Show Supplier Material materials with Elastic modulus of 10.8 GPa | dry | 1 mm | ISO 527-1/-2 | ||
11 GPa Show Supplier Material materials with Elastic modulus of 11 GPa | conditioned | ISO 527-1/-2 | ||||
11.3 GPa Show Supplier Material materials with Elastic modulus of 11.3 GPa | dry | ISO 527-1/-2 | ||||
11.5 GPa Show Supplier Material materials with Elastic modulus of 11.5 GPa | conditioned | ISO 527-1/-2 | ||||
120 °C | 8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | dry | ISO 527-1/-2 | |||
160 °C | 4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | dry | ISO 527-1/-2 | |||
200 °C | 4 GPa Show Supplier Material materials with Elastic modulus of 4 GPa | dry | ISO 527-1/-2 | |||
Elongation | 1.9 % Show Supplier Material materials with Elongation of 1.9 % | conditioned | ISO 527-1/-2 | |||
2 % Show Supplier Material materials with Elongation of 2 % | dry | ISO 527-1/-2 | ||||
2.4 % Show Supplier Material materials with Elongation of 2.4 % | dry, conditioned | 1 mm | ISO 527-1/-2 | |||
120 °C | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |||
160 °C | 5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-1/-2 | |||
200 °C | 5.5 % Show Supplier Material materials with Elongation of 5.5 % | dry | ISO 527-1/-2 | |||
Flexural modulus | 10.5 GPa Show Supplier Material materials with Flexural modulus of 10.5 GPa | dry | ISO 178 | |||
11 GPa Show Supplier Material materials with Flexural modulus of 11 GPa | conditioned | ISO 178 | ||||
80 °C | 10 GPa Show Supplier Material materials with Flexural modulus of 10 GPa | dry | ISO 178 | |||
120 °C | 7.5 GPa Show Supplier Material materials with Flexural modulus of 7.5 GPa | dry | ISO 178 | |||
160 °C | 4.5 GPa Show Supplier Material materials with Flexural modulus of 4.5 GPa | dry | ISO 178 | |||
200 °C | 4 GPa Show Supplier Material materials with Flexural modulus of 4 GPa | dry | ISO 178 | |||
Flexural yield strength | 260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | conditioned | ISO 178 | |||
290 MPa Show Supplier Material materials with Flexural yield strength of 290 MPa | dry | ISO 178 | ||||
80 °C | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | dry | ISO 178 | |||
120 °C | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |||
160 °C | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |||
200 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |||
Impact strength, Charpy notched | 23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | conditioned | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry | ISO 179/1eA | |||
Impact strength, Charpy unnotched | 23 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | conditioned | ISO 179/1eU | ||
23 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m² | dry | ISO 179/1eU | |||
Tensile strength | 170 MPa Show Supplier Material materials with Tensile strength of 170 MPa | conditioned | ISO 527-1/-2 | |||
190 MPa Show Supplier Material materials with Tensile strength of 190 MPa | dry | ISO 527-1/-2 | ||||
190 MPa Show Supplier Material materials with Tensile strength of 190 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
200 MPa Show Supplier Material materials with Tensile strength of 200 MPa | dry | 1 mm | ISO 527-1/-2 | at low thickness | ||
120 °C | 125 MPa Show Supplier Material materials with Tensile strength of 125 MPa | dry | ISO 527-1/-2 | |||
160 °C | 85 MPa Show Supplier Material materials with Tensile strength of 85 MPa | dry | ISO 527-1/-2 | |||
200 °C | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 3e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3e-07 1/K | dry | ASTM D696 | Parallel | |
5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5e-07 1/K | dry | ASTM D696 | Normal | ||
Glass transition temperature | 125 °C Show Supplier Material materials with Glass transition temperature of 125 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Heat deflection temperature | 305 °C Show Supplier Material materials with Heat deflection temperature of 305 °C | dry | ISO 75-1/-2 | 2 MPa | |
320 °C Show Supplier Material materials with Heat deflection temperature of 320 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 325 °C Show Supplier Material materials with Melting point of 325 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry, conditioned | IEC 60112 | |
Dielectric constant | 3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 60250 | 10GHz |
3.9 [-] Show Supplier Material materials with Dielectric constant of 3.9 [-] | dry | IEC 60250 | 1GHz | |
3.9 [-] Show Supplier Material materials with Dielectric constant of 3.9 [-] | conditioned | IEC 60250 | 10GHz | |
4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | conditioned | IEC 60250 | 1GHz | |
4.5 [-] Show Supplier Material materials with Dielectric constant of 4.5 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
5 [-] Show Supplier Material materials with Dielectric constant of 5 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 33 kV/mm Show Supplier Material materials with Dielectric strength of 33 kV/mm | dry, conditioned | IEC 60243-1 | |
Dissipation factor | 120 [-] Show Supplier Material materials with Dissipation factor of 120 [-] | dry | IEC 60250 | 10GHz |
140 [-] Show Supplier Material materials with Dissipation factor of 140 [-] | dry | IEC 60250 | 1GHz | |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | conditioned | IEC 60250 | 1GHz | |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | conditioned | IEC 60250 | 10GHz | |
280 [-] Show Supplier Material materials with Dissipation factor of 280 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | dry | ISO 294-4 | Parallel |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 110 | dry | - | 1.0 mm 1000 bar |
Viscosity number | 98 cm³/gr Show Supplier Material materials with Viscosity number of 98 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Audio Jack Connectors, Temperature Sensor, Speed Sensor, Positition Sensor | |
Certifications | Yellow Card Available | |