Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel molybdenum Steel
EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-5 Grade S355J2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-5 Grade S355K2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-3 Grade S460N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-3 Grade S460NL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S275M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S275ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S355M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S355ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S420M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S420ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S460M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S460ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10028-5 Grade P420M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten