Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Ferritischer Edelstahl
DIN 17440 Grade X3CrTi17 soft annealed (+A)Ferritischer Edelstahl
DIN 17440 Grade X6CrAl13 soft annealed (+A)Ferritischer Edelstahl
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-5 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMo18-15-4 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-5 quenched (+Q)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMo18-15-4 quenched (+Q)Ferritischer Edelstahl
EN 10088-1 Grade X6CrAl13 soft annealed (+A)