Kohlenstoffarmer Stahl
EN 10028-2 Grade P235GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235JR as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235J0 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Chromium Steel
ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Kohlenstoffarmer Stahl
EN 10025-2 Grade S185 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Kohlenstoffarmer Stahl
DIN 1629 Grade St 37.0 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1626 Grade USt 37.0 normalized or normalized formed (+N)